Background of the Invention
(1) Field of the Invention
The present invention relates to a method of fabricating capacitors of integrated circuits, and more particularly to the buried N+silicon-to-polysilicide capacitors with low voltage coefficient of capacitance(hereinafter referred as VCC) of high density ICs.
(2) Description of the Related Art
A mixed-mode circuit includes logic circuits and analog circuits. A capacitor is one of the most important devices in the mixed-mode circuit and the voltage coefficient of capacitance is a key parameter to determine the operation performance of a capacitor. For the actual application to the IC manufacture, the VCC value is generally demanded to be less than 100 ppm/V.
The definition of the voltage coefficient of capacitance is the partial derivative of capacitance relative to voltage per standard capacitance. Please refer to the following formula: ##EQU1##
For the early mixed-mode process, the VCC values of obtained capacitors are generally less than 50 ppm/V, and match the specification of IC manufacturers. However, in recent years, the cell amount of ICs has been enhanced significantly, and the packing densities of ICs have been increasing considerably. In order to achieve high packing density, the cell sizes of ICs cell must be shrunk. As the sizes of the capacitors become smaller, the capacitance values of the capacitors are decreasing and the VCC values are dramatically increasing, causing the performance problem.
FIG. 1 shows a cross-sectional view of a conventional buried N+silicon-to-polysilicide capacitor. The process steps are briefly described as follows: A silicon substrate 1 with field oxide isolations 2 is provided. A buried layer 5 is formed by doping N-type impurities into the substrate 1 as the bottom plate of the capacitor. A dielectric layer 6 is then formed by thermal oxidation for the capacitor, and then a polysilicon layer 7 and a polysilicide layer 8 are formed by the low pressure chemical vapor deposition (LPCVD) method in consequence. Finally the polysilicide layer 8 and the polysilicon layer 7 are partially etched in consequence, and then the top plate 9 of the capacitor is formed.
The wafer numbers 1-3 of FIG. 2a show the capacitors formed by the conventional process with plate size 100*100 .mu.m.sup.2 having VCC values between 132 and 334 ppm/V, all of which are much higher than the application standard value 100 ppm/V. The wafer numbers 1-3 of FIG. 2b show the capacitors formed by the conventional process with plate size 40*40 .mu.m.sup.2 having VCC values between 148 and 2538 ppm/V, which are also much higher than the application standard value 100 ppm/V.
The present invention discloses a new method to fabricate a buried N+silicon-to-polysilicide capacitor with low voltage coefficient of capacitance.
Summary of the Invention
Accordingly, it is a primary object of the present invention to provide a method of fabricating a buried N+silicon-to-polysilicide capacitor with low voltage coefficient of capacitance(VCC).
It is another object of the present invention to provide a capacitor structure with low VCC for mixed mode IC applications.
In accordance with the objects of this invention, there is shown a method of fabricating a IC's capacitor. A silicon substrate, having field oxide isolations which define a capacitor region, is provided. A buried conducting layer is formed by doping N-type impurities into the substrate as the bottom plate of the capacitor. A dielectric layer is formed by thermal oxidation for the capacitor, and then a polysilicon layer is formed by the low pressure chemical vapor deposition method. Thereafter, a thermal diffusion step is performed to dope phosphorus into the polysilicon layer at a temperature range from 800.degree. C. to 950.degree. C. After forming of a polysilicide layer by the low pressure chemical vapor deposition method, arsenic ions are then implanted into the polysilicon layer and the polysilicide layer, in order to increase the dopant concentration of the capacitor's top plate and thus lower the VCC value of the capacitor. Finally the polysilicide layer and the polysilicon layer are partially etched in consequence, and the top plate of the capacitor is formed.
Brief Description of the Drawings
The accompanying drawings forming a material part of this description, in which:
FIG. 1 is a cross sectional representation of the capacitor made by the conventional art.
FIG. 2a is a VCC comparison diagram between the conventional art and this invention about the capacitors with plate area 100*100 .mu.m.
FIG. 2b is a VCC comparison diagram between the conventional art and this invention about the capacitors with plate area 40*40 .mu.m.
FIG. 3 is a cross sectional view showing a bottom plate of the capacitor is formed, in accordance with the present invention.
FIG. 4 is a cross sectional view showing a dielectric layer is formed on the bottom plate of FIG. 3.
FIG. 5 is a cross sectional view showing a polysilicon layer is formed on the dielectric layer of FIG. 4.
FIG. 6 is a cross sectional view showing a polysilicide layer is formed on the polysilicon layer of FIG. 5.
FIG. 7 is a cross sectional view showing N-type ions are implanted into the polysilicon layer of FIG. 5 and the polysilicide layer of FIG. 6.
FIG. 8 is a cross sectional view showing a top plate of the capacitor is formed.
Description of the Preferred Embodiment
Referring now in detail to the drawings for the purpose of illustrating preferred embodiments of the present invention, the process for fabricating capacitors with low voltage coefficient as shown in FIGS. 3 to 8 comprises the following steps:
FIG. 3 shows a forming step of a buried layer in a silicon substrate 1 as the bottom plate of a capacitor. A silicon substrate, having field oxide isolation, is provided. A photo resist 3 is spread and then a capacitor region is defined. Thereafter, N-type ions 4 such as arsenic are implanted into the substrate at an energy level from 60 keV to 120 keV, and a dose in the range from 2E14 cm.sup.-2 to 5E15 cm.sup.-2, and the bottom plate of the capacitor is formed.
FIG. 4 shows a forming step of a dielectric layer 6 on said silicon substrate 1 for the capacitor. The dielectric layer is formed to a thickness of about 100-750 Angstroms by thermal oxidation at a temperature range from 750.degree. C. to 950.degree. C.
FIG. 5 shows a depositing step of a polysilicon layer 7 on the dielectric layer 6. The polysilicon layer is formed to a thickness of about 1000-2500 Angstroms by the low pressure chemical vapor deposition method. Thereafter, a thermal diffusion step is performed to dope phosphorus into the polysilicon layer at a temperature range from 800.degree. C. to 950.degree. C.
The purpose of the thermal diffusion is to lower the sheet resistance of the polysilicon layer 7, and the higher the dose, the lower the sheet resistance of the polysilicon is. The dose of the thermal diffusion is controlled to obtain the sheet resistance of the polysilicon layer 7 in a range of 30.OMEGA. per square to 50.OMEGA. per square.
FIG. 6 shows a depositing step of a polysilicide layer 8 on the polysilicon layer 7. The polysilicide layer 8 is formed to a thickness of about 1500-2500 Angstroms by the low pressure chemical vapor deposition method. The polysilicon layer 7 and the polysilicide layer 8 are prepared for being patterned as the top plate of the capacitor. The purpose of the polysilicide layer is to lower the resistance of the capacitor's top plate.
FIG. 7 shows a doping step, the most importance step of the present invention. Arsenic ions 4a are implanted into the polysilicon layer and the polysilicide layer at an energy level from 60 keV to 120 keV, and a dose in a range from 5E15 cm.sup.-2 to 1E16cm.sup.-2. The purpose of this step is to increase the dopant concentration of the capacitor's top plate and thus lower the VCC of the capacitor.
FIG. 8 shows a patterning step of the top plate 9 of the capacitor. After the capacitor region is defined, the polysilicide layer 8 and the polysilicon layer 7 are etched in consequence except the capacitor region.
The different VCC performances between the conventional art and the present invention are shown in FIG. 2a and FIG. 2b. FIG. 2a shows the VCC values of capacitors with plate size 100*100 .mu.m.sup.2. The wafer numbers 1-3 of FIG. 2a are formed by using the conventional art and the wafer numbers 4-6 are formed by the process according to the present invention. As shown in FIG. 2a, the VCC values of capacitors formed by using the conventional art are between 132 and 334 ppm/V, but the VCC values of capacitors formed by the process according to the present invention are only between 23 and 28 ppm/V. FIG. 2b shows the VCC values of capacitors with plate size 40*40 .mu.m.sup.2. The wafer numbers 1-3 of FIG. 2b are formed by using the conventional art and wafer numbers 4-6 are formed by using by the present invention. As shown in FIG. 2b, the VCC values of capacitors formed by using the conventional art are between 148 and 2538 ppm/V, while the VCC values of capacitors formed by using the present invention are only between 42 and 85 ppm/V.
Therefore, as shown in FIG. 2a and FIG. 2b, the present invention makes a great improvement about the performance of the capacitors, whose VCC values are much lower than the standard value 100 ppm/V.
The invention being thus described, it will be obvious that the same may be varied in many ways. Such variations are not to be regarded as a departure from the spirit and scope of the invention, and all such modifications as would be obvious to one skilled in the art are intended to be included in the scope of the following claims.