Field of the Invention
The present invention relates to MOSFET devices. Even more particularly, the present invention relates to MOSFET devices with a deep source and a deep drain (deep source/drain junctions) and a shallow source extension and a shallow drain extension (shallow source/drain extensions).
Background of the Invention
In the prior art, laser annealing is used in ultra-shallow junction for ULSI MOS transistors using a pre-amorphization implant (by Si.sup.+ or Ge.sup.+ or Xe.sup.+) to create a shallow amorphous silicon (a-Si) layer under the surface of a substrate. The prior art then placed a gate and spacers over the shallow source/drain extensions and then used a separate process to create the deeper source and drain. The shallow source/drain extensions were desirable to prevent punch through. The deeper source/drains were desirable to allow silicidation. The prior art required separate processes to produce shallow source/drain extensions and deep source/drain junctions.
It would be advantageous to create a deeper source and drain and shallower source/drain extensions in a single process.
Brief Summary of the Invention
It is an object of the invention to provide method of creating a deep source/drain and shallow source/drain extensions with a single laser annealing process and a single implantation process.
Accordingly, the foregoing object is accomplished by providing on a semiconductor wafer a gate stack with side spacers. The side spacers are etched so that a known thickness of the side spacers is left. An ion beam is used to implant Si.sup.+ or Ge.sup.+ or Xe.sup.+ to amorphize the silicon region, creating an amorphous region with two different depths. A high dose ion beam is then used to implant a dopant. An oxide layer is then deposited as a barrier layer, and then a metal layer is deposited to improve laser energy absorption. Laser annealing is used to melt the amorphous silicon region which causes the dopant to diffuse into the amorphous silicon region creating deep source/drain junctions and shallow source/drain extensions. Conventional techniques are then used to complete the transistor fabrication.
Other features of the present invention are disclosed or apparent in the section entitled: "DETAILED DESCRIPTION OF THE INVENTION."
Brief Description of Drawings
For a fuller understanding of the present invention, reference is made to the accompanying drawings wherein:
FIG. 1 is a cross sectional view of part of a silicon wafer and the first phase of a MOSFET on the silicon chip.
FIG. 2,is a cross sectional view of part of a silicon wafer with the MOSFET undergoing,/amorphization.
FIG. 3 is a cross sectional view of part of a silicon wafer with the MOSFET undergoing dopant implantation.
FIG. 4 is a cross sectional view of part of a silicon wafer with the MOSFET undergoing laser annealing.
Reference numbers refer to the same or equivalent parts of the present invention throughout the several figures of the drawing.
Detailed Description of the Invention and Best Mode of the Invention
FIG. 1 is a cross sectional view of part of a silicon wafer 10 and the first phase of a MOSFET 11 on the silicon wafer 10. The surface of the silicon wafer 10 forms a substrate 12 for the MOSFET 11. The first phase of the MOSFET 11 has a gate 17 placed on a gate oxide 19 placed on the surface of the substrate 12. Plasma-enhanced chemical vapor deposition (PECVD) is used to deposit oxide spacers. A plasma dry etcher is used to etch back the oxide to form the oxide spacers 15 adjacent to the gate 17 as shown in FIG. 1. The manufacture of the first phase of the MOSFET is according to conventional means.
A well-controlled wet chemical etching (such as spray etching) is used to further etch the oxide spacers 15 so that only a known thickness of the oxide film is left at the corner of the gate 17, gate oxide 19 and substrate 12, as shown in FIG. 2. A first ion beam 21 provides a stream of either Si.sup.+ or Ge.sup.+ or Xe.sup.+ ions, which creates shallow amorphous silicon regions 23 under the etched oxide spacers 15 and deep amorphous silicon regions 25 away from the etched oxide spacers 15. The oxide spacers 15 are thin enough to allow some of the ions from the first ion beam 21 pass through to the substrate 12, but are thick enough to absorb some of the energy from the ions in the first ion beam 21. The ions passing through the oxide spacers are slowed, so that they create the shallow amorphous regions 23 below the spacers 15. Ions that do not pass into the oxide spacers 15 and the gate oxide 19 are not slowed down or stopped and therefore create the deep amorphous regions 25.
The oxide spacer 15 is then etched away, using anisotropic plasma etching. A second ion beam 27 is used to implant a high dose dopant into the shallow and deep amorphous silicon regions 23, 25, as shown in FIG. 3. For an n-channel MOSFET, arsenic or phosphorous is used as the dopant. For a p-channel MOSFET, boron or boron trifluoride is used as the dopant.
Plasma-enhanced chemical vapor deposition (PECVD) is used to deposit an oxide film barrier layer 29 over the surface of the silicon wafer 10 and the gate oxide 19, as shown in FIG. 4. A metal layer 31, of such metals as titanium, titanium nitride, and tantalum, is sputtered over the oxide film barrier layer 29 to improve laser energy absorption. An excimer laser beam 33 is used to provide ultra-rapid annealing. The deep and shallow amorphous silicon regions 23, 25 are melted by the laser annealing causing the dopant to diffuse throughout the deep and shallow amorphous silicon regions 23, 25. The deep amorphous regions 25 become source/drain regions 35. The shallow amorphous regions 23 become source/drain extensions 37. The laser annealing causes complete activation of the dopant causing high conductivity in both the source/drain regions 35 and the source/drain extensions 37.
The metal layer 31 and the oxide film barrier layer 29 are removed, and the conventional MOSFET processing is done to form a transistor, including the silicidation of the source/drain junctions. Because the source/drain junctions are deep, they can be more easily silicidated.
In the specification and claims the terms deep amorphous regions and shallow amorphous regions are relative terms, mainly meaning that the deep amorphous regions are significantly deeper than the shallow amorphous regions due to the use of the spacers to slow ions from the ion beam for amorphization. Preferably the deep amorphous regions are more than twice as deep as the shallow amorphous regions. More preferably, the deep amorphous regions are between 3 to 4 times as deep as the shallow amorphous regions. An example of depths in the preferred embodiment, shallow amorphous regions may be from 20-40 nm in depth and deep amorphous regions may be from 60-160 nm in depth.
The present invention has been particularly shown and described with respect to certain preferred embodiments and features thereof. However, it should be readily apparent to those of ordinary skill in the art that various changes and modifications in form and detail may be made without departing from the spirit and scope of the inventions as set forth in the appended claims. The inventions illustratively disclosed herein may be practiced without any element which is not specifically disclosed herein.