The invention will now be explained in greater detail by means of the following description which is illustrated by the accompanying drawings, in which:
FIG. 1 is a sectional view of a part of a housing in accordance with the invention;
FIG. 2 is a sectional view of an alternative embodiment of the same part of the housing in accordance with the invention; and
The FIGS. 3A and 3B are sectional views of the same part of the housing in accordance with the invention and of the alternative embodiment at various stages of the manufacturing process.
Each of the Figures shows substantially a cross-sectional view through one half of the housing with the part not shown being symmetrical to the part shown as regards the arrangement of the elements forming the housing.
The sectional view of FIG. 1 shows that the housing in accordance with the invention comprises a ceramic substrate 120 whose central part supports an electronic device 130 and a multilayer circuit 110 which ensures the electric connections between the electronic device and the pins 2. A cap 141 which may be made of a ceramic material warrants the protection of the electronic device.
In accordance with an alternative embodiment of the housing as shown in FIG. 2, the cap consists of two parts, a spacer 150 and a cover 140.
Usually, the electronic device 130 is a very large scale integrated circuit (VLSI) which is provided on a semiconductor material and comprises a large number of input and output terminals 7. Presently, the number of terminals amounts to approximately 144. However, due to the increasing demand for ever more complex circuits, the number of terminals may rise to 300 in the near future.
The housing which contains the device is connected to an electronic assembly, generally a printed circuit board, either by means of a pin grid array socket or directly, by soldering the housing onto the board. In either case, the electric and mechanical connections are made by pins 2 which are introduced in holes 3 in the substrate 120, as shown in FIG. 3A.
The number of pins 2 is at least equal to the number of terminals 7 of the electronic device. The large number and the requirement of a minimum spacing to avoid short-circuits, when the housing is connected to an external device, render it impossible to place all the pins in line with one another. Consequently, they are distributed over various rows at the periphery of the substrate.
The connection between the metal pins 2 and the terminals 7 of the electronic device is ensured on the one hand by the network 110 of the conductors which are screen-printed on the substrate 120, and on the other by flexible metal wires 6, which connect the end 8 of the conductors to the said terminals 7.
The number of conductors which should reach 300, and the pitch between their ends 8 which is in the order of magnitude of one tenth of a mm, necessitate the use of several levels to form the screen-printed network 110. Consequently, each conductor level 10, 20, . . . comprises a part of the conductors which contact a part of the pins 2, and is separated from the next conductor level by an electrically insulating layer 15 which, moreover, may be provided with openings for interconnecting two contiguous conductor levels. The network as a whole thus forms a multilayer circuit.
In order to overcome the problems which are inherent in the type of multilayer circuit selected to produce the prior art housing, a new type of screen-printable material is used to produce the housing of the invention and a new production method is proposed.
In accordance with the invention, a conducting compound which can suitably be used to form a screen-printable ink for providing the conductor layers 10, 20, . . . comprises copper powder and a vitreous binder. The ink obtained by means of this compound may be fired in a non-oxydizing atmosphere, for example nitrogen, at a temperature lower than the melting temperature of copper.
A conducting compound which meets these requirements may be, for example, the compound described in GB-A-1,489,031 or the British patent specification No. 2,037,270.
On the other hand, the insulating compound which may suitably be used to form a screen-printable ink for providing the insulating layers 15, has at least one vitreous phase. The ink obtained by means of the compound may be fired in a neutral atmosphere, for example nitrogen, at a temperature which is suited for the ink used to form the conducting layers 10, 20, . . .
An insulating compound which meets these requirements may be, for example, the compound described in U.S. Pat. No. 4,152,282 or in U.S. Pat. No. 4,323,652.
The different compounds stated are very suitable for the manufacture of the housing in accordance with the invention because they meet the requirements, since their firing temperature in nitrogen ranges from 850.degree. C. to 950.degree. C. and they are compatible with each other. Besides, they have many advantages.
The copper-containing conducting layers thus obtained exhibit a very good electric conductivity of about 1.5 milliohms per square for conductors having a thickness of 20 .mu.m (20 microns).
The insulating vitreous-crystalline layers have a coefficient of thermal expansion which is very close to that of the ceramic substrate up to their firing temperature. Consequently, the housings obtained are perfectly flat. Due to the fact that the different layers forming the housings are free from mechanical stress, the yield is close to 100%.
It is to be noted however, that the composition of both the conducting and the insulating layers, as given by way of example, renders it necessary for the layers to be fired one by one. However, the low firing temperature and the low cost of the materials used make it possible to attain low manufacturing costs.
Preferably, an insulating-protective layer 101 is formed on the last conducting layer by means of a composition which may suitably be used to form a screen-printable ink having a vitreous phase, and which can be fired at a low temperature of about 550.degree. C. This firing process must be carried out in a non-oxydizing atmosphere. An insulating compound which meets the said requirements may be, for example, the compound described in U.S. patent application Ser. No. 745,734, now U.S. Pat. No. 4,684,543 (or EP-A-85200960.4).
In an example of an embodiment, each conductor layer is formed in one screen-printing operation and has a thickness of about 15 .mu.m after firing.
Each insulating layer, which separates two conducting layers, is formed in two steps including an intermediate firing process, and after the final firing the thickness amounts to approximately 40 .mu.m.
As shown in FIG. 3A, the holes 3 in the substrate 120 , into which the pins 2 are introduced, may be formed by different methods, such as by using a laser beam or by boring.
The latter method is to be preferred because of its simplicity and because the inner sides of the holes have the same surface condition as that of the substrate and, consequently, can be directly subjected to the metal-plating process which is necessary in view of the subsequent mounting of the pins.
Laser-boring, however, causes a superficial vitrification of the inner sides of the holes, thus forming a poorly adhering crackled layer. This layer may be removed, for example, by subjecting it to a thermal treatment. It is alternatively possible to deposit two layers of the metal described below on the inner sides of the holes, the first layer containing an increased amount of up to 10% by weight of the vitreous binder and the second layer containing a normal amount (approximately 2% by weight of the vitreous binder).
After a substrate has been provided with holes the metallization of the holes, using a copper-containing ink which is identical to or compatible with the ink used for the conducting layers 10, is carried out preferably, prior to the formation of the multilayer circuit. For this purpose, the screen-printable ink used for metallizing is, for example, diffused into the hole 3 by reflowing so as to cover the walls of this hole, after which the ink is fired. In the same process, screen-printed conducting rings 11 and 12 are provided around the holes 3 on each of the faces 121 and 122, respectively, of the substrate 120.
A metal area 31 on which the electronic device 130 is to be mounted, is provided to the central part of face 121 of the substrate, for example, by means of a copper-containing ink as stated above. The multilayer circuit is fabricated on the same face 121 around the electronic device and the shanks of the pins 2 project equally from the face 121. Such an arrangement makes it possible to leave free the second face 122 of the substrate, thus providing space for fitting a radiator which dissipates the heat produced by the electronic device and which adversely affects the service life of the components of the electronic device. The radiator is not shown in the Figures because it does not form part of the invention.
The protective cap of the electronic device may be formed from a hollow part 141, as shown in FIG. 1, or from a spacer 150 and a cover 140, as shown in FIG. 2.
Generally, fitting the cap 141 or the cover 140 is the last operation in the manufacture of the housing. But if the cap consists of two parts, the spacer 150 is fitted on the protective layer 101, by means of a layer 33 which is identical to or compatible with the layer 101, consequently this operation is carried out at a low temperature of approximately 550.degree. C. Thus, the use of a two-part housing excludes all but one method of fitting the pins, which method will be described later on in the text and according to which the temperature will not surpass 550.degree. C. because, preferably, the spacer 150 is fitted on the layer 101 prior to fitting the pins.
A different shape is proposed for the pins to avoid their being pulled out which may happen when, after the housing has been mounted, it is lifted from its base several times in succession, for example during testing of the electronic device. In accordance with the invention, the pins have the shape of a shank with a flat head, that is to say, the pin has about the shape of a nail with a flat head. The pin is introduced into the metallised hole 3 so that the flat head 1 rests on the second face 122 of the substrate with the diameter of the head 1 being superior to the diameter of the hole 3. The shank of the pin sufficiently projects from the face 121 to ensure, for example, that the housing is suitably fitted to its base or that the housing is suitably soldered to a printed board.
Due to their particular shape, the pins of the housing in accordance with the invention are highly resistant to extraction. A metal which is suitable for forming pins is, for example, iron-nickel-cobalt.
When the electronic device is fragile, as is often the case, the pins are soldered before the electronic device is mounted on its mounting area. Consequently, the mounting area 31 and the ends 8 of the conductors must be protected during the soldering process. This can be accomplished by applying a few drops of a synthetic-resin varnish which is resistant to the solder in question and which leaves no trace after it is removed, i.e. it must not obstruct the subsequent soldering of the elements.
Products suitable for this purpose are, for example, a varnish which can be peeled off or a co-polymeric varnish of methyl-butyl polymethacrylate which can be dissolved in acetone. These products may also be used to protect the finished housing during the time it is stored.
For actually fixing the pins on the prepared substrate, as described above, three methods are proposed by way of example. Each of the methods includes the previous tin-plating of the pins, for example, by electro-deposition.
In accordance with the first method, the pins are soldered using a (60/40) tin/lead solder which settles at the location 23, as shown in the FIGS. 1, 2 or 3B. This method comprises positioning of the previously tin-plated pins 2 in the holes 3, their retention using an assembling process which is not described because it does not form part of the invention, and fixing the pins using solder. This may be done by immersing the pins in a solder bath containing the above-mentioned tin/lead mixture, for 5 to 8 seconds at a temperature of 230.degree. C., using a non-activated flux. Another technique called "wave soldering" may also be used. After purifying the flux and removing the protective varnish from the metal areas, the base of the housing thus formed may be provided with the device 130, the connecting wires 6 and the protective cap 141 as shown in FIG. 1 where the cap is in one piece 141 or with the protective cap as shown in FIG. 2 where the cap is made of two component parts 140, 150.
Meanwhile, the metal coating of the holes 13 and of the rings 11 and 12 may be oxidized. If so, they must be treated prior to soldering the pins, which treatment for the removal of the oxide from the surface of the copper layers may be selected from the treatments known to those skilled in the art. Possible treatments are, for example, immersing the base of the housing in a solution containing 120 g/l of ammonium persulphate to which 5 g/l of sulphuric acid are added, rinsing in deionized water, drying in compressed air and subsequently in a nitrogen atmosphere in an oven at 80.degree. C.
In carrying out the subsequent operations necessary to finish the housing, the temperature at which the pins have been fixed must be taken into account.
This is the reason why in accordance with the first method of fixing the pins, the electronic device is mounted by bonding together its rear end and the copper mounting area, using a silver conducting-adhesive. The bonding process is carried out in an oven, in a nitrogen atmosphere to avoid oxidation of the copper.
Next, the gold wires 6 are provided which interconnect the terminals 7 and the ends 8 of the conductors. This wiring process may be carried out, for example, using an ultrasonic-soldering machine with or an ultrasonic-welding machine, the ends of the conductors being free of oxidation.
The last operation consists in providing the hollow cap 141 or the cover 140. When the first method of fixing the pins is used, this last operation consists of applying a prepolymerized epoxy adhesive on the edge of the cap or cover and fixing the relevant element by means of polymerization in a nitrogen atmosphere for 15 minutes at a temperature of 150.degree. C. Thus, a very good sealing of the cap is obtained.
The housing obtaining by this first method which includes the fixation of the pins using a tin/lead solder at a temperature of 230.degree. C. and the fixation of the cap using an epoxy adhesive, can only be mounted on the printed board through the use of the spacer called "pin grid array socket". Directly soldering the housing onto the printed board would require a second flow soldering process, i.e. for 5 to 10 seconds at a temperature of 240.degree. C. However, this temperature is higher than the melting temperature of the tin/lead solder when heated for the second time, which is 183.degree. C. Consequently, the solder used for soldering the pins, in accordance with the first method, is not resistant to the soldering process in which the housing is soldered directly onto the printed board.
For this reason, the present invention proposes a second and a third method of fixing the pins.
In accordance with the second method, an additional metal coating is applied to the copper rings 11 and 12 prior to the fixation of the pins, which metal coating is applied by screen-printing an ink which comprises a (10%/88%/2% by weight, respectively) a tin/lead silver alloy, and which contains an averagely active flux which is necessary to suitably moisten the copper. The flux is applied to each side of the substrate so that the supply of a sufficient amount of the alloy to properly fill-up the space 23 (FIGS. 1, 2 and 3B) between the inner side of the hole and the pin is ensured as well as to ensure the formation of fillets 21 and 22 between the pin and the rings. Re-melting is carried out in a conveyor oven, in a nitrogen atmosphere, for 20 to 40 seconds at a temperature of 320.degree. C. Consequently, the pins thus fixed are resistant to re-heating up to a temperature of 280.degree. C. without the risk of melting.
When this second method for the fixation of the pins is used, the housing in accordance with the invention may be soldered onto the printed board. Meanwhile, the electronic device, the wires and the cap are fixed as described with regard to the first method.
In accordance with the third method of fixing the pins, round preforms having approximately the same shape and dimensions as the rings 12 are fabricated using a 71.15%/28.1%/0.75% by weight, respectively, silver/copper/nickel alloy. This ternary alloy has a temperature interval between solidity and liquidity which ranges from 780.degree. C. to 795.degree. C., thus, the melting cycle is not critical. Each pin is inserted in the corresponding metallized hole with the round preform being interposed between the nail-shaped head 1 of the pin and the face 122 of the substrate. The soldering process is carried out at high speed in a conveyor oven for about 30 seconds. The joints obtained with the 0.09 mm thick preforms are of a very good quality.
In accordance with this third method for the fixation of the pins, the electronic device is fitted on the mounting area by re-melting a silicon-gold eutectic at a temperature of 420.degree. to 425.degree. C. The gold wires are fixed by the method described hereinbefore, subsequently, the cap is secured using a gold/tin solder at 350.degree. C., thus a hermetic sealing superior to that of the two other methods is ensured.
The different methods for the manufacture of the housing in accordance with the invention are described by way of non-limitative examples, however, other methods may be conceived without departing from the scope of the invention as defined in the appended Claims.