Brief Description of the Drawings
The present invention will be described with reference to the accompanying drawings, wherein:
FIGS. 1A through 1D are side view schematic drawings depicting the processing steps used to form a field effect transistor using a semiconductor on insulator process, as known in the prior art;
FIGS. 2A through 2D are side view schematic drawings showing one embodiment of the present invention; and
FIG. 3 is a graph showing the improved radiation hardness of the described embodiment over a similar structure formed using prior art techniques.
Detailed Description of the Drawings
FIGS. 2A through 2D are side view schematic drawings depicting processing steps in accordance with one embodiment of the present invention. Although the described embodiment is for the fabrication of a P channel field effect transistor, it should be recognized that any active device presently used in integrated circuitry can be fabricated using the techniques shown. For example, bipolar devices, diodes, resistors, capacitors of all sizes and conductivity types are compatible with the described process. In addition, although the described process uses a silicon substrate with oxygen implants, it is not to be construed as limiting the present invention to silicon device processes. For example, the implantation of aluminum into a Gallium Arsenide substrate may be used to provide a sufficient barrier for formation of semiconductor on insulator devices.
FIG. 2A describes the initial steps for fabricating a field effect transistor as shown in this embodiment. Crystalline silicon substrate 21 is usually an undoped substrate, but may be formed using any doping type. An oxygen implant is performed at an energy of approximately 150 keV, but energies as high as 200 KeV are used. The upper energy limit is presently a function of the upper limits of commercially available machinery and not incompatibility with the described process. The density of oxygen ions is approximately 2.2.times.10.sup.18 ions per centimeter squared, however, densities as low as 1.times.10.sup.18 ions per centimeter squared have been successfully used. The substrate is maintained at a temperature of approximately 400.degree. to 600.degree. to maintain the crystallinity of the silicon surface. Following this implantation, the prior art shows an annealing step of approximately 1275.degree. C. Using the present technique, this annealing step is omitted. The prior art teaches that omitting this annealing step will provide an epitaxial layer for device fabrication of unacceptable quality. We have discovered that this is incorrect, and in fact, the omission of this annealing step provides advantageous results.
Turning now to FIG. 2B, epitaxial layer 27 is grown by chemical vapor deposition on the surface of the structure of FIG. 2A. This epitaxial layer is grown to a thickness of approximately 2,000 Angstroms to combine with layer 25 of FIG. 2A to form layer 27 of FIG. 2B having a thickness of approximately 3,300 Angstroms.
An etch mask (not shown) is formed and patterned on the surface of epitaxial layer 27 and epitaxial layer 27 is etched using an orientation dependent etch such as a dilute solution of hydrazine, ethylene diamine or potassium hydroxide with isopropyl alcohol or catechol. The resulting structure is mesa 29 as shown in FIG. 2C.
The structure of FIG. 2C is subjected to thermal oxidation in an oxygen ambient at approximately 850.degree. C. for approximately 10 minutes to form a silicon dioxide layer 31 on the surface of mesa structure 29. A polycrystalline silicon layer (not shown) is then formed on the surface of this gate oxide layer to a thickness of approximately 4,500 Angstroms using low pressure chemical vapor deposition. This polycrystalline silicon layer is doped using POCl.sub.3 doping at 900.degree. C. for approximately 30 minutes. A photoresist layer is formed and patterned on the surface of the polycrystalline silicon layer to serve as an etch mask for the polycrystalline silicon layer. The polycrystalline silicon layer is then etched using a plasma etching process using an HCl/HBr plasma. The photoresist is removed and the polysilicon layer is used as an implantation mask for an implantation of boron ions at an energy of approximately 20 KeV and a density of approximately 3.times.10.sup.15 ions per centimeter squared. This ion implantation is then annealed at a temperature of approximately 900.degree. C. in an argon environment for approximately 60 minutes to form source region 35 and drain region 37. The resulting structure is transistor 39, as shown in FIG. 2D.
FIG. 3 is a graph showing the comparison of the soft error rate of a static random access memory fabricated using the prior art and the present invention. LET is linear energy transfer or the rate of energy loss by ionization of an ion particle passing through a semiconductor device.
The above description is provided by way of example and in no way limits the scope of the invention claimed. The scope of the invention is only limited by the claims appended hereto.
Technical Advantages
The described embodiment of the present invention provides a semiconductor on insulator structure having improved characteristics. The described structure provides semiconductive material having reduced carrier lifetime thereby reducing the susceptibility of integrated circuitry formed therein to single event upsets caused by radiation striking the semiconductive area.