Background of the Invention
There has been an ever increasing concern with limiting loss of life and damage to property from fires, both in connection with transportation and in stationary facilities.
In connection with rail transportation, for example, the Transportation Systems Center of the U.S. Department of Transportation developed proposed Guidelines for flame spread and smoke density, as measured by ASTM E-162 and E662, respectively, for all interior materials in fixed guideway vehicles. In the years since these standards were proposed, there has been improvement in the safety performance of such interior materials.
Two areas, however, were left without standards. There were no established standards to limit the amount of toxic off-gases and the standards permitted the acceptance of combustible materials which contributed significant fuel to fires. As a result, some products that conformed to the guidelines were nevertheless not totally satisfactory in a practical sense.
One material, which has been used for several years as a fire retardant material, is a silicone rubber foam that is a reaction product of a vinyl-terminated polysiloxane containing --Si(CH.sub.3).sub.2 O-- units and an organohydrogen siloxane polymer containing --Si(H)(CH.sub.3)O-- units. This material has demonstrated good fire retardance and excellent weatherability, aging and durability properties and could be formulated to be a low emitter of toxic gases under fire conditions. Its fire retardance, however, is not good enough to meet the guidelines of the mass transit industry which require a flame spread index not greater than 25 when tested in accordance with ASTM E-162.
Summary of the Invention
In accordance with the present invention, a thermally insulative fire block sheet having an elastomeric layer is provided which has a surface flammability flame spread index of zero at 20 minutes of exposure in accordance with ASTM E-162 and which is capable, in a thickness of 1/16 inch, of blocking a flame of 1900.degree. F. for more than an hour. The sheet comprises at least two layers. One layer, facing the direction of the expected flame, is a cured silicone foam rubber comprising the reaction product of a vinyl-terminated polysiloxane containing --Si(CH.sub.3).sub.2 O-- units and an organohydrogen siloxane polymer containing --Si(H)CH.sub.3)O-- units. The silicone rubber foam also contains alumina trihydrate.
The other layer is an attached, adherent flame resistant support layer for the silicone foam, and is preferably a glass cloth layer.
A glass cloth fabric that has been found to be useful is a plain weave fiberglass fabric with a mass of about 200 grams per square meter and a thickness of about 0.17 millimeters that is fabricated from lubricated continuous yarn filaments which are each composed of electrical grade glass having a filament diameter of about 0.009 millimeters and which are combined in a single strand as one ply having a strand weight of about 66 grams per 1000 meters.
The silicone rubber foam is a modification of the foam sold commercially by General Electric Company as RTF 762 Silicone Rubber Foam. The latter is described in Modic U.S. Pat. No. 4,418,157; granted Nov. 29, 1983; and further details are described in Modic U.S. Pat. No. 4,189,545, granted Feb. 19, 1980. The commercially available silicone rubber foam is made of two ingredients, labelled "A" and "B", as hereinafter described. The silicone rubber foam of this invention contains, as an additional ingredient, from about 30 to about 55 weight percent of alumina trihydrate.
Part A of the silicone rubber formulation contains a polymer having the formula: ##STR1##
Part A also contains a finely divided crystalline silica in an amount from about 10 to about 100 parts by weight based on 100 parts of vinyl-containing polysiloxane and preferably 20 to 25 parts by weight thereof.
In addition, as disclosed in U.S. Pat. No. 4,189,545, Part A contains from 1 to 250 parts per million of a platinum catalyst, preferably a complex of platinum and a vinyl-containing polysiloxane.
Part B of the silicone rubber formulation contains a polymer having the formula: ##STR2##
In accordance with this invention, alumina trihydrate is added to the silicone rubber, generally to Part A thereof before the blending thereof with Part. B. The preferred blending ratios for Parts A and B is from about 10 to about 16 parts by weight of Part B per 100 parts of Part A. The preferred blending ratio between Part A and the alumina trihydrate is from about 50 to 125 parts of alumina trihydrate per 100 parts of Part A.
When silicone foams are prepared at varying ratios (in parts by weight) of Parts A and B and the alumina trihydrate, the following results are obtained:
The alumina trihydrate generally contains about 65 weight percent of Al.sub.2 O.sub.3 and about 35 weight percent of bound water which is lost on ignition. Good results have been obtained with alumina trihydrate materials which have the following properties:
wherein the surface area is measured by Perkins-Elmer Shell Sorptometer, and wherein the light reflectance is measured with a photo-volt reflectometer Model 670.
While it is not desired to be bound by any theory of operation, it is believed that the alumina trihydrate component functions initially by absorbing heat, first from the decomposition of the hydrate to liberate water and by vaporization of the water. Thereafter, after removal of the water, it is believed that the alumina combines with the silicone to produce aluminosilicate ceramics having substantial heat resistance.
After exposure to high temperatures, the normally flexible and resilient silicone foam rubber becomes brittle and crumbly and would fall apart if the silicone rubber layer were not adhered to the support layer.
The support layer may be any cohesive layer of a heat resistant material, such as a fiberglass cloth, and particularly a plain weave fiberglass cloth having a mass of 6 ounces per square yard and a thickness of 0.0068 inches. The support layer may also be made of other heat resistant fibers, such as wool, aramid, or polybenzimidazole, or of blends of such fibers with each other or with glass fibers.
The support layer may also be rigid, rather than flexible for certain uses, and may thus comprise materials such as plywood or composition board.
The support layer may also be a continuous, flexible impervious flame resistant sheet, such as a sheet of aluminum foil.
The bonding between the silicone foam rubber layer and the support layer is believed to be essentially mechanical with the silicone foam rubber layer penetrating slightly into the interstices in the glass fabric, for example. When the supporting layer is smooth, it may be necessary in some cases to use an adhesive, such as an acrylic adhesive, to bond the silicone foam rubber to the supporting layer. However, with aluminum foil an adhesive is unnecessary.
Brief Description of the Drawings
The invention may be better understood by reference to the drawings in which:
FIG. 1 is a cross-sectional view of one embodiment of the fire block sheet of the invention;
FIG. 2 is a cross-sectional view of another embodiment of the fire block sheet of the invention;
FIG. 3 is a perspective of another embodiment of the invention designed for the protection of electrical conducting cables; and
FIG. 4 is a reduced scale cross-sectional view of electrical conducting cables wrapped in the embodiment of FIG. 3.
Detailed Description of the Invention
As shown in FIG. 1, the fire block sheet of this invention, in its simplest form, comprises a silicone foam rubber layer 12, having a thickness dimension "A", attached to a support layer 13, such as a layer of fiberglass cloth, having a thickness "B".
Dimension "A" is typically substantially greater than dimension "B", although dimension "B" may be greater for certain contemplated uses. For sale on continuous rolls, the entire thickness of the fire block sheet (A+B) is typically from about 1/16 to about 1/4 inch.
In the embodiment of FIG. 2, there is an intermediate layer 14, of a metallic foil such as aluminum foil, between layers 12 and 13, which have the same meanings as in FIG. 1. In this embodiment, the aluminum foil, being impervious and reflective, prevents heat transfer therethrough by convection and reflects much of the heat which could otherwise pass therethrough by radiation. In addition, it transfers heat laterally by conduction. The latter property is applicable for uses where the expected source of heat would be a point source, such as a cigarette, match or welding torch.
The embodiment of FIG. 3 is designed for the protection of electrical conducting cables. In an industrial plant, and particularly in a nuclear power plant, it may be necessary during a fire, or other overheating, to transmit electrical energy to sense the emergency or its location, or to transmit power to equipment designed to cope with the emergency. Damage to electrical cables during a fire could frustrate the operation of damage control precisely when it is most needed.
In the rectangular fire block wrapper 10 shown in FIG. 3, layers 12 and 13 represent silicone foam rubber and fiberglass cloth as in FIG. 1. Layer 16 is a thick layer of non-woven insulating material, such as glass wool, and layer 17 is another layer of fiberglass cloth. The layers are stitched together in a quilting pattern (partially shown on the surface of layer 12) by ceramic stitching 18. Wrapper 10 includes end margins 24 and side margins 26.
Attachment strips 19 and 21, together comprise a fastening means made up of flexible strips of synthetic material, hook and loop type filament faced fasteners of the type generally known by the trademark VELCRO.RTM., strip 19 being secured at one side surface of wrapper 10 at one end margin and strip 21 being secured at the opposite side surface of wrapper 10 at the other end margin.
FIG. 4 shows the application of the wrapping product of FIG. 3 as it is wrapped around two electrical conducting cables 22 and 23 while attachment strips 19 and 21 are attached to each other to produce a closure about the cables. Elements in FIG. 4 which are identical to those of FIG. 3 bear the same identification numerals.
The fire block sheet of this invention may be made by first mixing the A portion of the silicone foam [comprising a vinyl-terminated polysiloxane containing --Si(CH.sub.3).sub.2 O-- units] with an approximately equal weight of finely divided alumina trihydrate with a paddle or in a dough mixer. Mixing generally takes 5-7 minutes and is continued until uniformity is obtained.
Then, the B portion of the silicone foam (comprising an organohydrogen siloxane polymer containing --Si(H)(CH.sub.3)O-- units) is added to the mixture in an amount of about 14 parts by weight per 100 parts of the original A portion. The components are vigororously mixed for about 30-45 seconds until uniformity is obtained.
Meanwhile, a process assembly has been prepared by attaching two sheets of matte polyester film (e.g., the film sold under the trademark Mylar.RTM.), to each other along one edge to form a hinged construction. The assembly is placed horizontally opened at its hinge, and a sheet of fiberglass cloth is placed on one of the polyester sheets.
The above-described mixture is then immediately poured onto the fiberglass cloth on the lower of the two sheets of matte polyester film; and the upper sheet is then closed over the mixture and the sheets positioned horizontally with the upper sheet parallel to the lower sheet. A roller is passed over the outer surface of the upper polyester sheet to spread the mixture through the entire area between the polyester sheets and to compress the mixture to a desired thickness.
The material between the two polyester sheets is cured at room temperature for about 15-20 minutes and then in a 100.degree. F. oven for about 5 minutes. A foam is formed in the desired thickness which is laminated to the fiberglass cloth.
The two polyester sheets are then peeled off the opposite surfaces of the fiberglass/silicone foam laminate.
The silicone foam layer of the product is a soft, flexible, partially closed cell foam which generally has a density between about 27 and about 37 pounds per cubic foot.
Typical properties of the fire block sheet are as follows:
All of the foregoing tests were run on 1/16" fire block sheets of FIG. 1 except where otherwise specified.
The fire block sheets of this invention may be useful in the fabrication of seats and other furnishings in aircraft and in passenger railroad cars. They may also be useful in the manufacture of switch box shields, in the jacketing of power, signal and communication cables, in rail car underbody flooring, in power rail coverings and as fire barriers in busses in the rear above the rear axle and in front of the engine compartment.
The invention has been described with reference to its preferred embodiments. It will be understood, however, by those skilled in the art that modifications may be employed without departing from the scope of the invention as defined in the claims.