Field of the Invention
This invention has to do with an improvement in the epoxidation of propylene oxide with tertiary butyl hydroperoxide. More specifically, it has to do with processing of a by-product stream containing tertiary butyl alcohol as a by-product and conversion of the alcohol to isobutylene.
Background of the Invention
Pure propylene oxide is in demand for the preparation of urethane foams, for example. One of the most widespread procedures for producing propylene oxide has been the epoxidation of propylene. Typical processes are described in U.S. Pat. Nos. 3,350,422 and 3,523,956. When tertiary butyl hydroperoxide is used as the oxidizing agent, the desired propylene oxide is formed. Relatively minor quantities of acetaldehyde, propionaldehyde, acrylic aldehyde, acetone, methanol, hexenes, water, are formed, as well as tertiary butyl alcohol. Fractionation of the reaction product is required.
One of the more efficient agents for oxidizing propylene to propylene oxide is tertiary butyl hydroperoxide, because its reduction product, tertiary butyl alcohol, may be isolated and sold or recycled to reform tertiary butyl hydroperoxide by the following steps: ##STR1##
In the recovery of tertiary butyl alcohol for dehydration to isobutylene, the tertiary butyl alcohol is vaporized and this step has proven to be particularly troublesome. The crude tertiary butyl alcohol discharged as a product from the distillation of the epoxidation products contains impurities which polymerize. The polymers are deposited on heat exchange surfaces of the equipment employed to vaporize the tertiary butyl alcohol.
It is an object of the present invention to reduce the fouling of the heat transfer surface in the tertiary butyl alcohol vaporizer thereby increasing the on-stream time between cleanings.
Further, it is an object of the present invention to reduce the organic content of the waste water discharge from the propylene oxide manufacturing plant.
Another object is to soften the deposits on the heat exchanger surfaces in the tertiary butyl alcohol vaporizer so that such deposits are more easily removed.
Summary of the Invention
In accordance with the present invention, there is provided a process wherein the operating conditions of the tertiary butyl alcohol vaporizer are modified whereby a substantial quantity of the crude tertiary butyl alcohol input to the vaporizer is removed as unvaporized liquid purge.
Specific Embodiments of the Invention
Vaporizer fouling is believed to be caused by polymerization of the above-mentioned impurities in the crude tertiary butyl alcohol. At the vaporizer temperatures, as from about 300.degree. F. to about 400.degree. F., the organic impurities adhere to the heat exchange surfaces, are decomposed and are carbonized, thereby greatly decreasing the heat transfer efficiency and obstructing the passages in the heat exchanger until eventually the process must be shut down and the heat exchanger cleaned to remove all accumulated deposits.
In accordance with the present invention, the deposits on the heat exchanger surfaces of the vaporizer are reduced by altering the process conditions so that a maximum of about 85 weight percent of the tertiary butyl alcohol fed to the vaporizer is vaporized, and at least about 15, and preferably from about 20 to about 40, weight percent of the tertiary butyl alcohol is blown down (removed as a bottoms fraction from the vaporizer). More preferably, the vaporizer is operated so that from about 70 to about 80 weight percent of a crude tertiary butyl alcohol feed stock passes to the dehydration reactor and about 20 to about 30 weight percent of the feed stock is so blown down.
Table I gives the results of an analysis of the total effluent from a propylene oxide manufacturing plant under various conditions of operating the tertiary butyl alcohol vaporizer. The operating time between vaporizer shutdown and the character of the deposits built up within the vaporizer are also summarized in Table I.
The organic content of the plant effluent slowly decreases as the material blown down from the vaporizer is increased up to about 40 weight percent of the vaporizer input. Although a smaller weight percent of tertiary butyl alcohol is vaporized and passes to the dehydration reactor under the preferred operating conditions (20-30 weight percent unvaporized liquid purge), this can be compensated for by increasing the feed rate of the crude tertiary butyl alcohol to the vaporizer.
For a better understanding of the present invention, a discussion of the various process steps will be given in conjunction with the figures.
FIG. 1 is a flow diagram of propylene oxide manufacturing process including the isolation and recycling of tertiary butyl alcohol to form tertiary butyl hydroperoxide.
FIG. 2 is a flow diagram of the process of the present invention.
The process broadly shown in FIG. 1, and the operating parameters of that process, are described in detail in U.S. Pat. Nos. 3,351,635 and 3,523,956, the disclosures of which patents are incorporated herein by reference. The area of the present invention is that portion of FIG. 1 which is enclosed in dotted lines and is reproduced in FIG. 2.
In FIG. 2, a feed stream 10 containing tertiary butyl alcohol, particularly a crude tertiary butyl alcohol containing impurities identified above, at temperatures between 75.degree. F. and 200.degree. F., is introduced into a vaporizer 11 under controlled conditions whereby at least 15% and not more than about 40% of the feed is blown down through line 12 to the still 13 or to further purification via line 14. The vaporizer is operated at temperatures between about 300.degree. F. and about 500.degree. F., and preferably between 325.degree. F. and 400.degree. F. The tertiary butyl alcohol that is vaporized at temperatures between 325.degree. F. and 400.degree. F. is passed through conduit 15 into one or more dehydration reactors 16. The dehydration reactor catalyst can be a porous form of aluminum oxide of high surface area such as Alcoa's F-1, Activated Alumina, as shown and described in U.S. Pat. No. 3,665,048. The quantity of catalyst required is related to the temperature and feed rates at which the reaction occurs. Normally, between 0.5 and 10 parts by weight of alcohol are fed per hour per part by weight of catalyst. Preferably, the feed rate is such that 2 to 4 parts by weight of alcohol per hour are introduced to reactor 16 per part by weight of catalyst. The temperature within reactor 16 is maintained between 475.degree. F. and 775.degree. F. The pressure at which the reaction takes place is not critical and satisfactory results are obtained in the range between atmospheric pressure and 300 p.s.i.g. For ease in downstream separation of the isobutylene from other reaction products, it is preferred to operate reactor 16 with an inlet pressure of about 100 to 250 p.s.i.g.
The effluent from reactor 16 passes through line 17 into a caustic water scrubber column 18, wherein the crude isobutylene is separated from acidic compounds by action of caustic water passed to scrubber 18 through line 19. The caustic water generally contains less than about 5 weight percent (e.g. about 0.1%) of NaOH. Crude isobutylene from scrubber 18 passes overhead through conduit 20 to further distillation columns (not shown) wherein the isobutylene is further purified as required. The isobutylene is either sold or is recycled to form tertiary butyl hydroperoxide by the process discussed above, involving hydrogenation to isobutane followed by oxidation; this is illustrated by suitable process blocks in FIG. 1. Used caustic water stream 21 is passed to stripper 22 where light impurities are removed overhead through line 23. The bottom water-caustic stream 24 is recycled to column 18 via line 19 with a portion being purged via line 25. Overhead 23 from stripper 22 can be used as fuel.
Returning to distillation column 14, heavy materials are removed as a bottoms product through line 26 for disposal from the system.
FIG. 1 and the above discussion are exemplary of the major process equipment necessary for dehydrating tertiary butyl alcohol derived from the epoxidation of propylene with tertiary butyl hydroperoxide using the present disclosure. There are many valves and heat exchangers that are included in the process to increase efficiency of over-all operation. However, these are conventional and within the purview of those skilled in the art.
The advantages of the present invention are most apparent from the following examples which show by way of comparison the improvement resulting from increasing the quantity of non-volatile liquid purge from the vaporizer.
Example I (Comparative)
A stream of tertiary butyl alcohol (TBA) from still 13 containing 96 weight percent TBA and 4 weight percent of other material is fed to vaporizer 11. The vaporizer is operated at temperatures between 355.degree. F. and 365.degree. F. and at pressures varying from 207 p.s.i.g. to 223 p.s.i.g. About 8% of the feed stream is returned as a liquid purge to still 13 and about 92% of the feed stream is vaporized, heated and sent to the dehydration reactors 16 which are operated between 700.degree. F. and 750.degree. F. The liquid purge from stripper 22 contained 4625 population equivalents of organic wastes that were purged during this period. About 40,000 tons of feed were sent to vaporizer 11 prior to having to stop operation to clean the vaporizer due to a reduction in heat transfer. The polymeric foulant on the vaporizer tubes was a hard black material that was difficult to remove.
Example Ii
The purity of the feed TBA stream to the vaporizer was the same as in Example I and the vaporizer was operated over the same temperature and pressure range. However, the average liquid returned to distillation still 13 was 20% of the feed stream. Dehydration reactor conditions were maintained similar to those of Example I. The organic content of the purge liquid stream from stripper 22 was found to be 3125 population equivalents as an average during this operation. About 62,000 tons of feed were sent to vaporizer 11 prior to having to stop in order to clean this unit. The nature of the foulant on the tubes of the vaporizer was found to be a softer, more easily removed material than the polymeric material found in Example I.